Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.74 - 9.94 g/cc | 0.352 - 0.359 lb/in³ | |
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Density | 9.74 g/cc | 0.352 lb/in³ | |
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.75 g/cc | 0.352 lb/in³ | |
Lucas-Milhaupt BRAZE 559 Silver Based Cadmium Free Filler Metal Characteristics:Braze 559 is an intermediate temperature silver brazing alloy similar to Braze 541 (54 Ag, 40Cu, 5 Zn, 1 Ni). It has a rather long melting range (220EF/105EC) so that it will tend t.. |