Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.492 g/cc | 0.3429 lb/in³ | |
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy Silvaloy A56T has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some applications. .. |
|||
Density | 9.492 g/cc | 0.3429 lb/in³ | |
Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy Silvaloy A56T Flux Coated Rod has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on som.. |