Density 9.21 g/cc
0.333 lb/in³
Indium Corp. Indalloy 217 Silver Solder Alloy
Information Provided by Indium Corporation
Density 9.21 g/cc
0.333 lb/in³
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Density 9.21 g/cc
0.333 lb/in³
Indium Corp. Indalloy 111 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Density 9.21 g/cc
0.333 lb/in³
ATI Allvac® Nickelvac® H-B-2 UNS N10665 Nickel Superalloy
Vessels, pumps, valves, piping systems for the production of hydrochloric, sulfuric, acetic, and phosphoric acids.Property values are for samples in the metallurgical condition: 1600°F age.Informat..
Density 9.21 g/cc
0.333 lb/in³
Indium Corp. Indalloy 218 Silver Solder Alloy
Information Provided by Indium Corporation