Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.21 g/cc
0.333 lb/in³
Thermal Properties Metric English Comments
Melting Point 620 - 650 °C
1150 - 1200 °F
Solidus 620 °C
1150 °F
Liquidus 650 °C
1200 °F
Component Elements Properties Metric English Comments
Copper, Cu 22 %
22 %
Silver, Ag 56 %
56 %
Tin, Sn 5.0 %
5.0 %
Zinc, Zn 17 %
17 %