Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.72 g/cc | 0.315 lb/in³ | |
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy Description: MoldStar® 150 is a high-performance, beryllium-free copper alloy for the blow molding and injection molding industries. In addition to its high thermal conductivity, MoldStar® 150 off.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.250 in (6.4 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.250 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.500 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Weartech International WT-800 Cobalt Hardfacing & Wear Resistant Alloy Applications: Magnetic tape heads, valves, extruder barrelsInformation provided by Weartech International |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
CLAL-MSX NICLAL 48 Copper Alloy Description: Niclal 48 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.72 g/cc | 0.315 lb/in³ | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture.. |