Polymer Property : Density = 8.327 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.327 g/cc
0.3008 lb/in³
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy
Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du..