Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | at RT. |
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Density | 8.07 g/cc | 0.292 lb/in³ | |
Wall Colmonoy COLMONOY® 62 SA - Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides Description and Application: Hard nickel-chromium-boron alloy containing Chromium Carbides. Excellent abrasion and corrosion resistance. Finished by grinding.Method of Application: Spraywelder, Fu.. |