Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.027 g/cc | 0.2900 lb/in³ | |
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800 Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both .. |
|||
Density | 8.027 g/cc | 0.2900 lb/in³ | |
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Density | 8.027 g/cc | 0.2900 lb/in³ | |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Density | 8.027 g/cc | 0.2900 lb/in³ | |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |