Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.01 g/cc
0.289 lb/in³
Special Metals NIMONIC® Alloy 105
A precipitation-hardenable nickel-cobalt-chromium alloy with an addition of molybdenum for solid-solution strengthening. The relatively high aluminum content enhances both strength (through greater..
Density 8.01 g/cc
0.289 lb/in³
Wall Colmonoy COLMONOY® 56 PTA - Nickel-Base Hard-Surfacing Alloy With Chromium Boride
Description: Colmonoy 56 PTA is a premium alloy specially formulated for plasma transferred arc (PTA) application on new and worn extrusion screws. High levels of chromium and carbon produce large ..