Physical Properties Metric English Comments
Density 7.901 g/cc
0.2854 lb/in³
American Elements Gadolinium Nanoparticles
General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp..