Material Notes:
General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 75 - 90 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Gadolinium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for gadolinium nanocrystals has focused on use in magnetic resonance imaging (MRI) by targeting coated gadolinium particles at tumors in an attempt to detect or label early stage cancer, particularly breast cancer, for Neutron Capture Therapy and for MRI Contrast Enhancement, as a dopant in glass and for their potential electrical, dielectric, magnetic, optical, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.
Physical Properties Metric English Comments
Density 7.901 g/cc
0.2854 lb/in³
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
0.075 - 0.090 µm
0.075 - 0.090 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 157.25 g/mol
157.25 g/mol
Thermal Properties Metric English Comments
Melting Point 1312 °C
2394 °F
Boiling Point 3250 °C
5880 °F
Descriptive Properties Value Comments
Appearance Black
Stability Moderately reactive in air
Users viewing this material also viewed the following: