Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.68 g/cc | 0.277 lb/in³ | |
Indium Corp. Indalloy 103 Tin-Cadmium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.68 g/cc | 0.277 lb/in³ | Coating Property |
The NanoSteel® Company SHS 9172 TWAS Steel Alloy, Cored Wire Coating Description: SHS 9172 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional wear, corrosion and high temperature oxidation resistance in severe abrasion.. |
|||
Density | 7.68 g/cc | 0.277 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9192 GMAW OAW Steel Alloy, Cored Wire Coating Description: SHS 9192 GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features extreme abrasion resistance with high toughness, high volume of har.. |
|||
Density | 7.68 g/cc | 0.277 lb/in³ | |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Density | 7.68 g/cc | 0.277 lb/in³ | |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Density | 7.68 g/cc | 0.277 lb/in³ | |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |