Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.67 g/cc | 0.277 lb/in³ | |
Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10) Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles w.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Latrobe 440â„¢ N-DUR High Quality Martensitic Stainless Steel 440 N-DUR is a 15.0% chromium stainless steel that provides the corrosion resistance of 440 C with the added benefit of improved carbide size and distribution for noiseless miniature precision beari.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze Finished product available as bar, rod, forged or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extr.. |
|||
Density | 7.67 g/cc @Temperature 191 °C |
0.277 lb/in³ @Temperature 375 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 40 HRC |
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic.. |
|||
Density | 7.67 g/cc @Temperature 400 °C |
0.277 lb/in³ @Temperature 752 °F |
hardened to 58 HRC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
Density | 7.67 g/cc @Temperature 200 °C |
0.277 lb/in³ @Temperature 392 °F |
|
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
|
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Density | 7.67 g/cc @Temperature 400 °C |
0.277 lb/in³ @Temperature 752 °F |
|
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Density | 7.67 g/cc @Temperature 400 °C |
0.277 lb/in³ @Temperature 752 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Density | 7.67 g/cc @Temperature 400 °C |
0.277 lb/in³ @Temperature 752 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735 AL 29-4C alloy is a superferritic stainless steel designed by Allegheny Ludlum for extreme resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking, as well as general cor.. |
|||
Density | 7.67 g/cc @Temperature 399 °C |
0.277 lb/in³ @Temperature 750 °F |
|
Assab Steels 8407 SUPREME Hot Work Steel 8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and .. |
|||
Density | 7.67 g/cc | 0.277 lb/in³ | |
Lucas-Milhaupt HANDY HI-TEMP 095 Carbide Brazing Alloy Applications:Handy Hi-Temp 095 is a ductile copper-nickel-manganese filler metal designed for intermediate temperature brazing of carbides, cast irons, steel, stainless steels and nickel base heat-r.. |