Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AL 29-4C alloy is a superferritic stainless steel designed by Allegheny Ludlum for extreme resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking, as well as general corrosion in oxidizing and moderately reducing environments. The alloy was developed in the early 1980s for welded condenser tubing to be used in seawater and brackish water by the power generation industry. It is this extreme resistance to pitting and crevice corrosion that has led to the installation of over 2000 miles of AL-29-4C tubing in power plant condensers and heat exchangers.The superferritic stainless steel AL 29-4C alloy shows excellent resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking. This resistance makes it an ideal choice for battling the corrosive condensate of partially and fully condensing natural gas and propane burning appliances. Its low alloy content, compared to other high-performance alloys, makes it an economical choice as well.Property data below is typical of annealed samples. Information provided by Allegheny Ludlum.
Physical Properties Metric English Comments
Density 7.67 g/cc
0.277 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Tensile Strength, Ultimate 655 MPa
95000 psi
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
Elongation at Break 22 %
22 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 29 %
29 %
Iron, Fe 65 %
65 %
as balance
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 4.0 %
4.0 %
Nickel, Ni 0.30 %
0.30 %
Niobium, Nb (Columbium, Cb) 0.60 %
0.60 %
includes Ti
Nitrogen, N 0.020 %
0.020 %
Phosphorous, P 0.030 %
0.030 %
Silicon, Si 0.35 %
0.35 %
Sulfur, S <= 0.010 %
<= 0.010 %
Users viewing this material also viewed the following: