Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.56 g/cc | 0.273 lb/in³ | |
Assab Steels VANADIS 4 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di.. |