Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.273 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.57 g/cc
0.273 lb/in³
MarkeTech NB:WO (Sodium Bismuth Tungstate, NaBi(WO4)2) Scintillator Crystal
Double tungstate of sodium and bismuth NaBi(WO4)2 (NBWO) is also a new "heavy", "fast" and optically dense oxide single crystal. Is used as a Cherenkov radiator.Data provided by the supplier, MarkeT..
Density 7.57 g/cc
0.273 lb/in³
MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.2%.
Density 7.55 g/cc
0.273 lb/in³
Indium Corp. Indalloy 118 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Density 7.57 g/cc
0.273 lb/in³
Ferro EG 2791 Thick Film Glass
Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co..
Density 7.57 g/cc
0.273 lb/in³
Mateck Neodymium Gallate Substrate, NdGaO3
Substrate single crystals for superconductivity
Density 7.55 g/cc
0.273 lb/in³
Williams Advanced Alloys WS213 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.56 g/cc
0.273 lb/in³
Assab Steels VANADIS 4 Cold Work Steel
VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di..
Density >= 7.55 g/cc
>= 0.273 lb/in³
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric
Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used ..
Density >= 7.55 g/cc
>= 0.273 lb/in³
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric
Navy Type ICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens..
Density >= 7.55 g/cc
>= 0.273 lb/in³
Channel Industries 5804 Lead Zirconate Titanate Piezoelectric
Navy Type IIICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exte..