Polymer Property : Density = 7.455 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.455 g/cc
0.2693 lb/in³
Crucible Steel CPM® 9V® Tool Steel
CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced..