Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.455 g/cc | 0.2693 lb/in³ | |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |