Polymer Property : Density = 6.95 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.95 g/cc
0.251 lb/in³
Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy
FormaMet is an aluminum bronze cold working die alloy used for the drawing or forming of stainless steel, low carbon steel and other materials. When used for deep drawing and forming applications of..