Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 6.51 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.51 g/cc
0.235 lb/in³
MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
Density 6.51 g/cc
0.235 lb/in³
Mateck Lanthanum Aluminate Substrate, LaAlO3 cubic
Substrate single crystals for superconductivity
Density 6.51 g/cc
0.235 lb/in³
Mateck Lanthanum Aluminate Substrate, LaAlO3 rhombohedral
Substrate single crystals for superconductivity
Copyright © lookpolymers.com All Rights Reserved