Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.55 g/cc | 0.128 lb/in³ | |
Schott N-SK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.55 g/cc | 0.128 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |