Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.54 g/cc | 0.128 lb/in³ | |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Density | 3.53 g/cc | 0.128 lb/in³ | |
Schott N-SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.55 g/cc | 0.128 lb/in³ | |
Schott N-SK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.54 g/cc | 0.128 lb/in³ | |
Schott N-SK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.53 g/cc | 0.128 lb/in³ | |
Schott N-SSK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.53 g/cc | 0.128 lb/in³ | |
Schott N-SF57HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.55 g/cc | 0.128 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |