Polymer Property : Density = 3.50 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.00 - 3.50 g/cc
0.0361 - 0.126 lb/in³
Average value: 1.08 g/cc Grade Count:174
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Density 0.882 - 3.50 g/cc
0.0319 - 0.126 lb/in³
Average value: 1.06 g/cc Grade Count:387
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..