Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 3.33 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.33 g/cc
0.120 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 601 Mullite
Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e..
Density 3.33 g/cc
0.120 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton EXP 338 Alumina 99.6%
EXP 338 features high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cyc..
Density 3.33 g/cc
0.120 lb/in³
ICE Hot Pressed SiC
Data provided by the manufacturer, International Ceramic Engineering.
Density 3.33 g/cc
0.120 lb/in³
Schott N-BAF51 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.33 g/cc
0.120 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
Density 3.33 g/cc
0.120 lb/in³
ASTM-C20
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
Density 3.33 g/cc
0.120 lb/in³
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride
Uniform, large sized pressed sintered aluminum nitride.
Density 3.33 g/cc
0.120 lb/in³
ASTM-C20
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..
Copyright © lookpolymers.com All Rights Reserved