Physical Properties Metric English Comments
Density 3.281 g/cc
0.1185 lb/in³
Reade Advanced Materials Diopside Powder (CaMg(CO3)2 and CaMg(SiO3)2)
Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings.Forms Available: Lum..