Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.281 g/cc | 0.1185 lb/in³ | |
Reade Advanced Materials Diopside Powder (CaMg(CO3)2 and CaMg(SiO3)2) Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings.Forms Available: Lum.. |