Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.03 g/cc | 0.109 lb/in³ | |
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | |
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0303 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityAppearance: Natural Color and WhiteInformation provided by TP Composites, Inc... |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | |
3M Nextel™ 550 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural applications w.. |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | |
3M Nextel™ CF-40 Woven Fabric 550 Information provided by 3M |
|||
Density | 3.03 g/cc | 0.109 lb/in³ | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |