Polymer Property : Density = 2.73 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.73 g/cc
0.0986 lb/in³
Raw material (not vacuum-formed products)
ICHS Fiberfax® Alumina-Silica Ceramic Fibers
Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C..
Density 2.73 g/cc
0.0986 lb/in³
Schott BG39 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Density 2.73 g/cc
0.0986 lb/in³
Fiber Density
Zircar Ceramics ASBF Alumina-Silica Bulk Fiber
Type ASBF Alumina-Silica Bulk Fiber is long alumina-silica fibers suited for the vacuum forming of low density shapes, for use as packing or as a bulk fill material. It is useful to temperatures of ..
Density 2.73 g/cc
0.0986 lb/in³
Fiber Density
Zircar Ceramics ASBF-1 Alumina-Silica Bulk Fiber
Type ASBF-1 Alumina-Silica Bulk Fiber is a specially processed fiber which has low shot content and relatively short fiber length. Suitable for vacuum forming of rigid boards & shapes in a range of ..
Density 2.73 g/cc
0.0986 lb/in³
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..