Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.73 g/cc | 0.0986 lb/in³ | Raw material (not vacuum-formed products) |
ICHS Fiberfax® Alumina-Silica Ceramic Fibers Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C.. |
|||
Density | 2.73 g/cc | 0.0986 lb/in³ | |
Schott BG39 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.73 g/cc | 0.0986 lb/in³ | Fiber Density |
Zircar Ceramics ASBF Alumina-Silica Bulk Fiber Type ASBF Alumina-Silica Bulk Fiber is long alumina-silica fibers suited for the vacuum forming of low density shapes, for use as packing or as a bulk fill material. It is useful to temperatures of .. |
|||
Density | 2.73 g/cc | 0.0986 lb/in³ | Fiber Density |
Zircar Ceramics ASBF-1 Alumina-Silica Bulk Fiber Type ASBF-1 Alumina-Silica Bulk Fiber is a specially processed fiber which has low shot content and relatively short fiber length. Suitable for vacuum forming of rigid boards & shapes in a range of .. |
|||
Density | 2.73 g/cc | 0.0986 lb/in³ | |
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |