Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.37 g/cc | 0.0856 lb/in³ | |
Pyrotek Pyrocast ZG Refractory Shapes Aggregate Base: FireclayApplicationsDoor sill Door lintel Door jamb Information provided by Pyrotek. |
|||
Density | 2.37 g/cc | 0.0856 lb/in³ | |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Density | 2.37 g/cc | 0.0855 lb/in³ | |
ITW Devcon Metal Repair Titanium Putty, Grey Information provided by ITW Devcon |
|||
Density | 2.37 g/cc | 0.0856 lb/in³ | |
Schott FG3 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG13 |
|||
Density | 2.37 g/cc | 0.0856 lb/in³ | ASTM D792 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |