Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.25 - 2.35 g/cc | 0.0813 - 0.0849 lb/in³ | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |