Polymer Property : Density = 17.6 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 17.6 g/cc
0.636 lb/in³
MarkeTech 93-4-3 Tungsten Alloy, AMS-T-21014 Class 2
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Density 17.6 g/cc
0.636 lb/in³
Wieland 1703 Wilaform Gold
Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Density 17.6 g/cc
0.636 lb/in³
Goodfellow Platinum 70/Rhodium 30 Thermocouple Alloy
Information provided by Goodfellow.