Polymer Property : Density = 15.92 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 15.92 g/cc
0.5751 lb/in³
Indium Corp. Indalloy 196 Gold Solder Alloy
Information Provided by Indium Corporation