Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.7 g/cc | 0.459 lb/in³ | |
China Tungsten YT535 Tungsten Carbide Wear resistance red hardness better than YT540 and high strength in use. Continuous rough turning and milling of cast or forged steelInformation provided by China Tungsten |
|||
Density | 12.7 g/cc | 0.459 lb/in³ | |
China Tungsten ZP35 Tungsten Carbide A versatile grade High in red hardness, strength in use and resistance to impact and thermal shocking. Roughing and strength cutting of steel and cast steel.Information provided by China Tungsten |
|||
Density | 12.7 g/cc | 0.459 lb/in³ | |
Cadi 20TC Tungsten Carbide Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Density | 12.7 g/cc | 0.459 lb/in³ | |
Cadi TCWA Tungsten Carbide Copper Alloy Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |