Polymer Property : Density = 12.33 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 12.33 g/cc
0.4454 lb/in³
Wall Colmonoy COLTUNG 1 Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
Description and Application: A nickel-chromium-boron matrix alloy rich in chromium boride is used to hold extremely hard tungsten-carbide particles. Produces rod-welded deposits with same chemistry..