Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Tungsten Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLTUNG
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLTUNG 1 Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description and Application: A nickel-chromium-boron matrix alloy rich in chromium boride is used to hold extremely hard tungsten-carbide particles. Produces rod-welded deposits with same chemistry as spray-applied Colmonoy® Nos. 75 or 705. Finished by grinding. Information provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 12.33 g/cc
0.4454 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58 - 63
58 - 63
Component Elements Properties Metric English Comments
Boron, B 1.9 %
1.9 %
Carbon, C 1.75 %
1.75 %
Chromium, Cr 7.0 %
7.0 %
Cobalt, Co 0.12 %
0.12 %
Iron, Fe 2.2 %
2.2 %
Nickel, Ni 45.88 %
45.88 %
As Balance
Silicon, Si 2.65 %
2.65 %
Tungsten, W 38.5 %
38.5 %
Processing Properties Metric English Comments
Processing Temperature 1040 °C
1900 °F
fusing temperature