Polymer Property : Density = 11.26 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 11.26 g/cc
0.4068 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
Density 11.26 g/cc
0.4068 lb/in³
CMW® ELKONITE® TC5 Tungsten Carbide Copper material
For wiping and arcing electrical contacts and light duty welding tips.Information provided by CMW Inc.