Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.26 g/cc | 0.4068 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Density | 11.26 g/cc | 0.4068 lb/in³ | |
CMW® ELKONITE® TC5 Tungsten Carbide Copper material For wiping and arcing electrical contacts and light duty welding tips.Information provided by CMW Inc. |