Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.44 - 1.91 g/cc | 0.0520 - 0.0690 lb/in³ | |
Parker Chomerics CHO-SHIELD® 4076-50A Conductive Coating Conductive Nickel-Filled Coating. This is an electrically conductive waterborne nickel-filled polyurethane coating that provides excellent shielding against radiated EMI. It bonds well to plaster, c.. |
|||
Density | 1.22 - 1.91 g/cc | 0.0441 - 0.0690 lb/in³ | Average value: 1.47 g/cc Grade Count:89 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |