Physical Properties Metric English Comments
Density 1.514 g/cc
0.05470 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp WFB51 PBT
LNP THERMOCOMP* WFB51 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Glass Fiber. Added features of this material include: Low Warpage.This data was supplied by SABIC-..