Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.475 g/cc @Temperature 120 °C |
0.05329 lb/in³ @Temperature 248 °F |
|
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |
|||
Density | 1.475 - 1.49 g/cc | 0.05329 - 0.0538 lb/in³ | ISO 1183 |
Tisan TISMOSET® Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti.. |