Polymer Property : Density = 1.424 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.424 g/cc
0.05145 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC
LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing.
Density 1.424 g/cc
0.05145 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Density 1.424 g/cc
0.05145 lb/in³
DIN 53 479
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Density 1.424 g/cc
0.05145 lb/in³
Melt; ISO 1183
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in..