Polymer Property : Density = 1.333 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.333 g/cc
0.04816 lb/in³
crystalline density; SABIC (IRC0032)
SABIC HC 050 Amorphous Polyethylene Terephthalate
Product Description: HC 050 is an amorphous, low molecular weight thermoplastic PET made by a continuous melt-phase polymerization process.Characteristics: HC 050 is a specially formulated amorpho..
Density 1.333 g/cc
0.04816 lb/in³
ISO 1183
Stir SpA AF 68 FR (PVC)
Application: Extrusion flame resistant sheath with high resistance to low temperaturesInformation provided by STIR SpA