Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.333 g/cc | 0.04816 lb/in³ | crystalline density; SABIC (IRC0032) |
SABIC HC 050 Amorphous Polyethylene Terephthalate Product Description: HC 050 is an amorphous, low molecular weight thermoplastic PET made by a continuous melt-phase polymerization process.Characteristics: HC 050 is a specially formulated amorpho.. |
|||
Density | 1.333 g/cc | 0.04816 lb/in³ | ISO 1183 |
Stir SpA AF 68 FR (PVC) Application: Extrusion flame resistant sheath with high resistance to low temperaturesInformation provided by STIR SpA |