Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.278 g/cc | 0.04617 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66 LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare |