Physical Properties Metric English Comments
Density 1.215 g/cc
0.04389 lb/in³
ISO 1183
Stir SpA B 3001 S AT (PVC)
Application: Molding for ecological boot-legInformation provided by STIR SpA
Density 1.215 g/cc
0.04389 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.
Density 1.215 g/cc
0.04389 lb/in³
ISO 1183-1
Covestro Makrolon® 1954 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosity• UV st..
Density 1.215 g/cc
0.04389 lb/in³
3M Scotchcast™ 2130 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it..
Density 1.215 g/cc
0.04389 lb/in³
BorsodChem ONGRONAT T 65 TDI 65/35 Isocyanate
Description of product:Appearance: At room temperature water clear liquid.Composition: A mixture of toluene diisocyanate isomers (2,4-toluene diisocyanate [A] and 2,6-toluene diisocyanate [B]. Nomin..