Polymer Property : Density = 1.109 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.109 g/cc
0.04007 lb/in³
Melt Density
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur..
Density 1.109 g/cc
0.04007 lb/in³
Latex
DuPont Performance Polymers Neoprene 115 Polychloroprene  (discontinued **)
Main feature: Mechanical stability methacrylic acid copolymer reactive. Principal uses include: Coatings, Modifiers, Asphalt, Concrete.Solids content: 47%. Initial pH: 7. Surface tension: 47 dyne..