Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.101 g/cc | 0.03978 lb/in³ | |
CRP Technology Windform® XT Polyamide-Carbon Composite WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with .. |
|||
Density | 1.101 g/cc | 0.03978 lb/in³ | |
Dow Hydroxyethyl Acrylate Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |