Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.074 g/cc | 0.03880 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8103 EP BLK Ash is 24.7%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.074 g/cc | 0.03880 lb/in³ | ASTM D792 |
North Wood Plastics PS with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |