Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 8103 EP BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8103 EP BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ash is 24.7%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.074 g/cc
0.03880 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0093 cm/cm
0.0093 in/in
ASTM D955
Melt Flow 1.1 g/10 min
1.1 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
10 sec; ASTM D-2240
Tensile Strength, Ultimate 4.30 MPa
624 psi
ASTM D412
Elongation at Break 406.1 %
406.1 %
ASTM D412
Flexural Modulus 0.0567 GPa
8.22 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 33.5 kN/m
191 pli
ASTM D624